在使用山東自動(dòng)焊接設備的時(shí)候,總會(huì )出現一些故障,為了解決這一難題,一般要根據具體情況加以解決處理。下面來(lái)講講自動(dòng)焊接設備焊接鋼件抗壓強度不足的解決。
When Shandong automatic welding equipment is used, there will always be some failures. In order to solve this problem, it is generally necessary to solve it according to the specific situation. Now let's talk about how to solve the problem of insufficient compressive strength of steel parts welded by automatic welding equipment.
(1)檢查水平的壓力是否過(guò)小,檢查水平條是否能夠固定。
(1) Check whether the horizontal pressure is too small and whether the horizontal bar can be fixed.
(2)檢查焊接能量是否太小,焊接鋼是否生銹,焊點(diǎn)是否差。
(2) Check whether the welding energy is too small, whether the welding steel is rusty, and whether the welding spot is poor.
(3)檢查電頭和電梯桿、電梯桿和電梯臂之間是否有過(guò)剩的化合物。
(3) Check whether there is any excess compound between the electric head and the elevator pole, elevator pole and elevator arm.
(4)檢查電氣級頭的斷面是否因破損而增加,減少焊接能量。
(4) Check whether the section of the electrical connector is increased due to damage to reduce welding energy.
(5)檢查電級和銅軟聯(lián)和融合面可否焦慮不安空氣氧化。
(5) Check whether the electrical level, copper soft joint and fusion surface can be oxidized by anxious air.
如果出現點(diǎn)焊強度不足問(wèn)題,那么需要檢查電極壓力是否過(guò)小,焊接工件的外觀(guān)是否存在腐蝕或鐵銹現象,檢查電極頭與電極棒、電極棒與電極臂是否有過(guò)多的氧化物。
If the spot welding strength is insufficient, it is necessary to check whether the electrode pressure is too low, whether the appearance of the welding workpiece is corroded or rusted, and whether the electrode head and electrode rod, electrode rod and electrode arm have too much oxide.
提醒您,在平時(shí)做好對設備的保養維護工作,避免問(wèn)題的出現。以上就是詳細為您介紹問(wèn)題具體的內容,以供大家參考運用。關(guān)注我們http://www.aplwebs.com,了解更多!
Remind you to do a good job of equipment maintenance at ordinary times to avoid problems. The above is a detailed introduction to the specific content of the problem for your reference. Follow us http://www.aplwebs.com , learn more!